Classification of Aluminum Corrosion
From the perspective of corrosion morphology, aluminum corrosion can be divided into general corrosion and localized corrosion. The former is also called uniform corrosion, or overall corrosion, which refers to the material surface in contact with the environment being uniformly corroded and worn. Corrosion of aluminum in alkaline solutions is a typical example of uniform corrosion, such as during alkaline cleaning, where the aluminum surface thins at approximately the same rate and the mass decreases. However, it should be noted that absolute uniform corrosion does not exist, as the thinning varies in different areas. Localized corrosion refers to corrosion occurring in specific regions or parts of a structure, and it can be further divided into the following categories:
1. Pitting Corrosion
Pitting corrosion occurs in extremely localized areas or spots on the surface of a metal, forming pits or holes that expand inward, and can even cause perforation. When the pit opening is smaller than the depth of the pit, it is called pitting corrosion; when the pit opening is larger than the depth, it can be called crater corrosion. In practice, there is no strict boundary between pitting and crater corrosion. Aluminum experiencing corrosion in an aqueous solution containing chlorides is a typical example of pitting corrosion. Pitting corrosion is the most common form of aluminum corrosion and is caused by a potential difference in a certain region of the aluminum compared to the base metal, or by the presence of impurities with a potential different from that of the aluminum matrix.
2. Intergranular Corrosion
This type of corrosion is a selective corrosion that occurs at the grain boundaries of a metal or alloy without significant attack on the grains or crystals themselves. It can cause a severe reduction in the mechanical properties of the material, potentially leading to structural damage or accidents. The cause of intergranular corrosion is that under certain conditions, grain boundaries are highly reactive. For example, impurities may exist at the grain boundaries, or the concentration of a certain alloying element may increase or decrease at the grain boundaries. In other words, there must be a thin region at the grain boundary that is electrochemically negative relative to the rest of the aluminum, which preferentially corrodes. High-purity aluminum can undergo this type of corrosion in hydrochloric acid and high-temperature water. Al-Cu, Al-Mg-Si, Al-Mg, and Al-Zn-Mg alloys are all sensitive to intergranular corrosion.
3. Galvanic Corrosion
Galvanic corrosion is also a characteristic form of aluminum corrosion. When a less active metal and a more active metal, such as aluminum (anode), come into contact in the same environment or are connected by a conductor, a galvanic cell is formed, causing the flow of current, which leads to galvanic corrosion. Galvanic corrosion is also known as bimetallic corrosion or contact corrosion. Aluminum has a very negative natural potential, so when it contacts other metals, aluminum always acts as the anode, accelerating corrosion. Almost all aluminum and aluminum alloys cannot avoid galvanic corrosion. The greater the potential difference between the two metals in contact, the more severe the galvanic corrosion. It is particularly important to note that in galvanic corrosion, the area factor is crucial; a large cathode with a small anode is the most unfavorable combination.
4. Crevice Corrosion
When the same or different metals come into contact, or metals contact non-metals, crevices can form, leading to corrosion within or near these crevices. There is no corrosion outside the crevice, which is caused by the lack of oxygen inside the crevice, leading to the formation of a concentration cell. Crevice corrosion is almost independent of the type of alloy; even highly corrosion-resistant alloys can suffer from it. The acidic environment at the crevice tip is the driving force behind corrosion. This type of corrosion occurs under deposits or fouling, such as the under-deposit corrosion on the surface of 6063 aluminum alloy construction profiles under gray paste, which is a very common form of deposit-induced crevice corrosion. Flange connections, nut fastening surfaces, overlapping surfaces, weld pores, areas under rust layers, and deposits such as sludge, scale, and impurities on the metal surface can all trigger crevice corrosion.
5. Stress Corrosion Cracking
Stress corrosion cracking is corrosion cracking caused by the coexistence of tensile stress and a specific corrosive medium. The stress can be external or residual stress within the metal. Residual stress may arise from deformation during manufacturing, sudden temperature changes during quenching, or volume changes caused by internal structural changes. Stresses from riveting, bolting, press-fitting, or shrink-fitting are also residual stresses. Stress corrosion cracking occurs when the tensile stress on the metal surface reaches the yield strength Rpo.2. Thick plates of 2000 and 7000 series aluminum alloys develop residual stress during quenching and should be relieved by pre-stretching before aging treatment to prevent deformation during aircraft component processing or to avoid transferring stress into the parts.
6. Lamellar Corrosion
This type of corrosion, also known as delamination, flaking, or layered corrosion, can be simply referred to as exfoliation. It is a special form of corrosion found in 2000, 5000, 6000, and 7000 series alloys, and is commonly seen in extruded materials.
7. Filiform Corrosion
This is a type of corrosion that can develop in a worm-like pattern under the paint or other coatings on aluminum materials, but it has not been observed under anodized films. It generally occurs under the coatings of aircraft aluminum structural components and architectural or structural aluminum parts. Filiform corrosion is related to the material composition, pretreatment before coating, and environmental factors. Environmental factors refer to temperature, humidity, chlorides, and the like.