Jan 31, 2026 Leave a message

Ten Issues To Pay Attention To in The Production Of Two-Color Aluminum Profiles

(1) Choose a film with moderate width and thickness; due to the complex cross-sectional shapes of aluminum profiles, the surface varies significantly between wide and narrow areas, which can easily cause the edges to lift and reduce the film's coverage, affecting the painting quality. If the film is too narrow, it won't cover adequately, making spraying obviously impossible. On the other hand, when selecting the film thickness, as long as it provides coverage and is elastic, it is sufficient; there is no need to choose a film that is too thick, as overly thick film increases the production cost of aluminum profiles and is unnecessary.

(2) Spray painting promptly after applying the film. After the profile is covered with film, painting should be done promptly, with shorter waiting times being better. If the waiting time is too long, the adhesive on the film will dry and lose its stickiness. If exposed to wind, the film may peel off, making painting difficult. Therefore, to ensure both the film and painting quality, the waiting time after applying the film generally should not exceed 16 hours.

 

(3) Choose a protective film with moderate viscosity. In the processing and production of two-color aluminum profiles, selecting the right protective film is crucial. If the film's viscosity is too low, it won't stick properly, making it easy to peel off, which significantly complicates the spraying process. If the film's viscosity is too high, it means there is too much adhesive on the film; when the film is removed, the adhesive can stick to the profile, affecting the surface quality. Additionally, when selecting a protective film, it is best to use one whose adhesive composition is the same as or close to that of the paint, which can help minimize the impact on the paint's color.

 

(4) Determine the color, boundary surfaces, and boundary lines. Before spraying aluminum profiles, it is essential to identify the color to be applied on each surface according to the profile's function and the customer's requirements, determine which surfaces are the boundary surfaces, which lines are the boundary lines, and their positions. Generally, the inside is a light color and the outside is a dark color. Only after clarifying the boundary surfaces, boundary lines, and color requirements can the protective film be applied, and it is crucial not to place the film in the wrong position.

 

(5) Film quality: Applying film is a key process in the processing of two-color aluminum profiles. The quality of the film directly affects the surface quality of the aluminum profiles, and mainly includes the following aspects: First, when applying the film, try not to create excessive tension in the film, meaning the film should not deform. Otherwise, the applied film is prone to shrinkage, causing the ends of the aluminum profiles to have uncoated areas. On the other hand, when the film at the ends of the aluminum profile is disconnected, it should be cut with a blade rather than pulled apart, because a pulled film will still shrink. Second, the film width should match the coating width. Generally, the film width should be slightly larger than the width of the aluminum profile surface. If the film is too wide, extending too far beyond the edge of the profile, it can be lifted by compressed air during spraying. If the film is too narrow and cannot fully cover the surface, it is obviously not acceptable. Fourth, when the surface boundary is at the edge of a groove, the excess film must be pressed into the groove, otherwise, airflow during spraying can lift the film, affecting the spray coating quality. Fifth, when applying the film, it should be applied smoothly to prevent wrinkles or curling. Sixth, for profiles with complex cross-sectional shapes, if applying the film all at once is difficult, it can be done in two or more steps to ensure full coverage. Seventh, for special profiles with thin walls or large cantilevered sections, the film should not be applied too tightly to avoid deforming the aluminum profile. Eighth, after the first spraying, the aluminum profile should not be left standing for too long, otherwise dust may settle on the surface, making it difficult to apply film and affecting its quality.

 

(6) Strictly implement the film application process. When applying film to aluminum profiles, it must be done after the first coating. Directly applying the film after chromating the profile is not allowed because the film has adhesive. If the film is applied directly to the chromated layer, the adhesive may stick to the chromated layer, or peeling off the film could remove the chromated layer. This will greatly reduce the paint film's adhesion, ultimately affecting the spraying quality of the aluminum profile and causing paint peeling, with potentially serious consequences.

(7) Timing of film removal. After aluminum profiles have been film-applied and sprayed, the film needs to be removed. However, it should not be removed immediately after spraying; proper timing must be controlled. Generally speaking, after spraying, a leveling process occurs until the paint film is basically solidified, which should take no less than 10 minutes before the film can be removed. Otherwise, if the paint film hasn't set, peeling off the film may leave residues on the aluminum profile and affect the paint quality. Additionally, the film should be removed quickly to avoid compromising the quality of peeling.

(8) Avoid repeated rework. In the production of two-color aluminum profiles, rework is sometimes unavoidable due to various factors. However, each rework requires another curing process. For the paint film, multiple coatings increase the thickness, and repeated curing weakens the adhesion, making the paint prone to peeling. Therefore, in the production of two-color aluminum profiles, multiple reworks should be avoided whenever possible.

 

(9) Reasonable control of film thickness: The production of two-color aluminum profiles requires more than one coat of spraying. If we operate as if it were a single spray, it will result in some finishes being too thick and others too thin, causing severe unevenness in film thickness. Therefore, spraying should be reasonably controlled. During the first spray, only the main areas of one side need to be sprayed, while the other side can be left unsprayed or lightly sprayed. The second spray, called a flash coat, should focus as much as possible on the required areas, with little or no spraying on other areas. At the same time, the thickness of the second spray should be reasonably controlled based on the first spray and the color of the paint used, while ensuring that the second spray effectively covers the first spray.

 

(10) For two-color coating of aluminum profiles, two colors need to be applied. Among the two colors, there is always a darker and a lighter color. The spraying process must follow a sequence, so it is necessary to consider which color to spray first and which to spray later based on the specific situation. If the lighter color is sprayed first and the darker color later, the first-applied lighter color will need to undergo two curing processes, meaning it will be baked twice, which can easily cause the light color to discolor. If the darker color is sprayed first and the lighter color later, the coverage of the first-applied darker color by the subsequent lighter color will be somewhat affected; achieving full coverage of the dark color would require increasing the coating thickness. However, if the coating becomes too thick, it can lead to peeling. Therefore, in actual production, the process of spraying light color first and then dark color is more feasible.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry