Mar 04, 2026 Leave a message

Aluminum Electrolytic Cell Roasting Start-up Technology

2.1 Comparison of Several Technologies for Starting Prebaked Electrolytic Cells

Both domestically and abroad, large-scale prebaked aluminum electrolytic cells commonly adopt the method of preheating and starting with furnace lining. Specifically, there are four technical methods: aluminum bath startup, coke particle startup, graphite startup, and gas startup.

In domestic prebaked cells, the most commonly used method for commissioning and starting is the traditional aluminum bath startup technique. Its greatest advantage is its simplicity in operation, with uniform temperature rise in later stages and easy control. In recent years, with the third wave of aluminum electrolysis construction in China and the development towards larger electrolytic cells (200 kA to 300 kA).

 

2.2 Control of the Three Heating Stages in Preheating and Baking of Prebaked Aluminum Electrolytic Cells

2.1.1 Low-Temperature Preheating Stage

The average temperature of the lining in the cell should be controlled below approximately 200°C. The main purpose of controlling the temperature during this period is to remove moisture from the lining material, while also slowing down the thermal expansion deformation between the cathode carbon blocks, binder, cathode steel bars, and the cell shell during the initial stage of baking. This reduces the damaging effect on the lining caused by differences in thermal expansion coefficients among various materials. Especially below 200°C, the plasticity of the cathode steel bars is very low, while their thermal expansion coefficient is about 3–4 times that of the cathode carbon blocks. Proper control of the temperature rise rate will prevent early cracking of the cathode carbon blocks. During this period, the heating rate should generally be controlled at about 5°C per hour.

 

2.2.2 Medium-Temperature Roasting Stage

During this period, the temperature is controlled within the range of approximately 200℃ to 600℃. The purpose is to remove volatile substances and crystalline water from the lining material. At this time, the cathode steel rod has changed from thermal expansion deformation to creep deformation (the yield point of steel is 200℃), increasing its plasticity. The main task during this period is to roast the binding paste in the gaps between cathodes and around the slot edges, thereby improving the bonding performance between the binding paste and the cathode carbon blocks. During this period, the heating rate can reach 10–20℃ per hour.

2.2.3 High-Temperature Coking Stage

The temperature is around 600℃. This period involves high-temperature roasting of the side lining. The purpose of temperature control is to ensure that the cathode carbon blocks and the binding paste are fully bonded and coked into a single piece, reaching the conditions required for normal production. It is important to note that after the temperature reaches 500℃, the binding paste undergoes free expansion due to coking and then transforms into shrinkage deformation. At this time, the cathode carbon blocks still remain in the expanded deformation state. Therefore, the binding paste around the slot edges will likely develop some shrinkage cracks. It is necessary to promptly control the heating rate.

Send Inquiry