Causes and solutions of metal beans, burrs and triangles on the surface of aluminum alloy profiles

Causes and solutions of metal beans, burrs and triangles on the surface of aluminum alloy profiles

The surface of the metal bean --- aluminum alloy profile is attached to the spherical gray-black hard particle metal, and the structure is loose. On the surface of the aluminum alloy profile, there are two kinds of energy and non-erasure.
The burr (triangular mouth) --- the pits formed by the enlarged black hard particle metal after rubbing the surface of the aluminum alloy profile and during the friction, lifting and falling of the same flowing profile.

 

Causes of aluminum defects: 

(1): The alloy composition of the aluminum rod, the high amount of silicon Si and the amount of iron Fe, and the improper ratio of magnesium Mg and silicon Si (the silicon content exceeds the standard value), the excess silicon and iron will be more active than the performance of aluminum metal, and the magnesium atoms are separately grabbed in the Al-Mg-Si crystalline phase and combined into magnesium 2 silicon Mg2Si phase and aluminum-iron-silicon phase ALFeSi, which makes the grain coarse and needle-like structure, with active performance, increased hardness and poor plasticity. Most of these metal beans can be rubbed (alkali washed) off
(2): The hardness of the working belt in the aluminum extrusion die is not enough, the dead angle is too large, the use is too long, and the working belt is too long.
(3): The aluminum extrusion speed and extrusion temperature are too fast and too high, and the aluminum rod is too long and the surface aluminum is pressed in.
(4): The fit between the pad and the pad, the pad and the cylinder is out of tolerance, and the metal beans are often deeply embedded in the surface of the aluminum profile and can not be wiped off (alkali washing).

(5): Adsorption of external debris and air dust.

(6): During production, the hot rod is baked too early, the surface temperature of the aluminum rod drops, and the grain precipitation is coarse, so special attention should be paid to the production of cemented carbide.

 

Elimination:

The key to the elimination of metal beans of aluminum alloy profiles lies in the quality of aluminum rods, and the high iron content of silicon is the main problem of granular metal on the surface. In the process of aluminum production, the matching between pads and pads, pads and cylinders is out of tolerance, so that the relatively stable attached surface aluminum in the extrusion cylinder is destroyed, and the attached surface aluminum with the same cylinder temperature (about 400 degrees) is significantly lower than the extrusion rod temperature slowly peeled off from the cylinder wall with the friction between metals, forming fine, low-temperature, slightly higher hardness ALFeSi metal particles, which are pressed into the surface of the profile when passing through the die hole, forming metal beans that cannot be wiped off by hand.

 

Another reason encountered: Changfa Aluminum 630 tons of production of 6061 rim material surface coarse burrs are serious, the rod replacement is ineffective, the production of 6063 is not, and it was found that the cylinder phase temperature is only 365 degrees, and the 390 degree extrusion profile burrs disappear after repair. The reason is that the extrusion speed of 6061 rim material is slow, and the precipitation of magnesium 2 silicon Mg2Si phase and aluminum-iron-silicon phase ALFeSi is concentrated on the surface of the aluminum rod during the heat transfer and cooling process between the outer layer of the rod (520 degrees) and the cylinder wall, which is reflected on the surface of the profile through the dead zone.

After shearing and pressing, the die surface is uneven, and metal beans are easy to appear on the surface of the profile.

If the quality of the rod is very poor, and the fit between the pad and the pad, the pad and the cylinder is seriously incompatible, the metal beans will be coarse, and the hole will be stacked at the outlet of the working belt when extruded from the die, and the surface of the aluminum alloy profile will be attached or scratched on the surface of the profile, forming burrs (triangular mouths) on the surface of the profile.

 