Several methods to improve the yield of aluminum extrusion

How to improve extrusion yield? There are the following suggestions for extrusion operators and extrusion inspectors:
1) Quality inspection: machine quality inspection should take fast, accurate and ruthless inspection methods, the so-called "fast" is the inspection diligent and timely; "Quasi" is to be familiar with national standards, internal control standards, different customers and different surface treatment standards, when necessary to sample the corresponding surface treatment test, there must be no misjudgment and excessive acceptance phenomenon in special circumstances can not determine to immediately report to the relevant person in charge; "Ruthless" is the stance and implementation of the enforcement of institutional majesty.
2) Extrusion monitor: can not pull the wrong mold, can not write the wrong tracking card, to actively do a good job of quality self-inspection and process inspection.
3) Host operator (acting monitor) : Actively cooperate with the work of the monitor, verify each set of molds, control the three temperatures, flexibly grasp the flow rate of the material according to the structure of different models and different surface treatment, check the quality of the material at any time, responsible for the wall thickness, forming degree, impact collapse drag and or internal drag, accurately calculate whether the material head after sawing into semi-finished products of different specifications and varieties is long enough.
4) Interrupted work: interrupted work is also a very important position, find quality problems to tell the monitor or the monitor for the first time, each set of mold machine out to check the height of the lifting frame and graphite block and high temperature roll is intact, because they will directly affect the forming degree of the material, open the fan in time to check whether the conveyor belt transport process is smooth and effective. If it is found that the surface of the profile has steam bubble oil bubble, flushing collapse and drag, it is necessary to make a clear mark on the profile to prevent the flow into the next process.
5) Straightening workers (compounding, sizing sawing, framing workers) :
Each material in the adjustment of the surface quality to a comprehensive check, can not make the cold bed of the profile pile too much, so as to avoid rubbing, hollow profiles to choose the appropriate plug head to prevent excessive deformation of the broken head. If there is an assembly relationship, the sample of the corresponding surface treatment model in this batch order shall prevail, so as to control the drawing rate of straightening.
When combining materials, pay attention to different surface treatment materials have different combining methods, billets, oxidizing sandblasting materials, "oxidizing electrophoretic light fabric" as far as possible to the non-decorative side down or non-decorative surface and non-installation face together, keep the interval between the branches of the profile and the decorative surface as far as possible to avoid rubbing, touching, scratching, scratching, damage.
Before cutting, consider whether the material head and tail waste are long enough, if the whole material or batch is not long enough, immediately notify the interruption or boot hand, and carefully check whether the end of the profile is deformed after sawing, such as the sawing deformation can be adjusted to slow down the sawing speed.
Thermal insulation materials (the order specifically indicates the strict acceptance of bending and twisting according to customer requirements, and the order does not indicate the acceptance of high precision) must be framed before each piece of material passes the platform before it can be framed, the shape is more complex after framing the profile that the partition strip is easy to crush should be separated by each layer flat tube, the product with strict surface quality requirements should be separated by a single branch of high temperature felt, and the partition strip must be placed neatly.